Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 1.00e+17 ohm @Temperature 23.0 °C |
1.00e+17 ohm @Temperature 73.4 °F |
ASTM D257 |
DuPont™ Nomex® Type 993, 120 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Surface Resistivity per Square | 1.00e+17 ohm @Temperature 50.0 °C |
1.00e+17 ohm @Temperature 122 °F |
ASTM D257 |
DuPont™ Nomex® Type 993, 120 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Surface Resistivity per Square | 1.00e+17 ohm @Temperature 100 °C |
1.00e+17 ohm @Temperature 212 °F |
ASTM D257 |
DuPont™ Nomex® Type 993, 120 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |