Electrical Properties Metric English Comments
Surface Resistance 0.0014 ohm
0.0014 ohm
12K
Hexcel® HexTow™ IM6 Carbon Fiber
HexTow™ IM6 carbon fiber is a continuous, high performance, intermediate modulus, PAN based fiber available in 12,000 (12K) filament count tows. The fiber has been surface treated and can be sized ..