Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 0.0300 - 1.00e+12 ohm | 0.0300 - 1.00e+12 ohm | Average value: 3.13e+10 ohm Grade Count:21 |
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max.. |