Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.10e+11 - 1.00e+15 ohm | 1.10e+11 - 1.00e+15 ohm | Average value: 1.44e+14 ohm Grade Count:8 |