Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Surface Resistance = 1.26e+12 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 1.26e+12 ohm
1.26e+12 ohm
ASTM D257
Tipco Tipcolite® THD 411 Phenolic Compound, Mica, Asbestos & Cellulose, Medium Flow & High Electrical Properties
Medium Flow Phenolic Compound, Reinforced with Mica, Asbestos & CelluloseApplications: Electrical & ElectronicsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industr..
Copyright © lookpolymers.com All Rights Reserved