Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | >= 1.60e+14 ohm | >= 1.60e+14 ohm | ASTM D257 |
3M Scotch-Weld™ DP820 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |