Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 150 ohm | 150 ohm | ASTM D257 |
Saint-Gobain Meldin® 1003 Thermoplastic Bearing Material Meldin 1003 components offer the highest level of strength and rigidity for this product family. They maintain high chemical, tensile, and flexural properties even at elevated temperatures.MeldinÂ.. |