Polymer Property : Surface Resistance = 2.00e+14 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 2.00e+14 ohm
2.00e+14 ohm
Test 2
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin
Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a..
Surface Resistance 2.00e+14 ohm
2.00e+14 ohm
ROA; IEC 60093
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East)
VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..
Surface Resistance 2.00e+14 ohm
2.00e+14 ohm
Covestro Baydur® 40 Polyurethane
Rigid integral skin polyurethane foam for lightweight moldings. Sandwich structure gives a high stiffness-to-weight ratio.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience ..
Surface Resistance 2.00e+14 ohm
2.00e+14 ohm
cond; IEC 60093
DSM Novamid® 1010C2 PA6
Easy Molding Grade
Surface Resistance 2.00e+14 ohm
2.00e+14 ohm
cond; IEC 60093
DSM Novamid® 1010GH30 NAT PA6-GF30
30% Glass Reinforced, Heat Stabilized, Injection Molding
Surface Resistance 2.00e+14 ohm
2.00e+14 ohm
cond; IEC 60093
DSM Novamid® 1010N2 1ES NAT PA6 FR(30)
Injection Molding, Flame Retardant (Halogen free)
Surface Resistance 2.00e+14 ohm
2.00e+14 ohm
cond; IEC 60093
DSM Novamid® 1011CH5KR PA6
Heat Stabilized, Easy Molding Grade
Surface Resistance 2.00e+14 ohm
2.00e+14 ohm
cond; IEC 60093
DSM Novamid® 1013C5 PA6
Injection Molding, Easy Molding Grade
Surface Resistance 2.00e+14 ohm
2.00e+14 ohm
cond; IEC 60093
DSM Novamid® 1013G30 1 NA PA6-GF30
30% Glass Reinforced, Injection Molding
Surface Resistance 2.00e+14 ohm
2.00e+14 ohm
cond; IEC 60093
DSM Novamid® 1013GH30 1 NA/BK701 PA6-GF30
30% Glass Reinforced, Heat Stabilized, Injection Molding
Surface Resistance 2.00e+14 ohm
2.00e+14 ohm
cond; IEC 60093
DSM Novamid® 1015G33-8 NAT PA6-GF33
33% Glass Reinforced, Injection Molding
Surface Resistance 2.00e+14 ohm
2.00e+14 ohm
IEC 60093
DuPont Performance Polymers Hytrel® 4053FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Surface Resistance 2.00e+14 ohm
2.00e+14 ohm
Reliance Industries PVAXX H60
The key property of all PVAXX polymer is this product`s unique capacity to biodegrade into non-toxic residues under both aerobic and non-aerobic conditions.Information provided by Reliance Industrie..
Surface Resistance 2.00e+14 ohm
2.00e+14 ohm
Test 2
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin
Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a..