Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 2.00e+17 ohm | 2.00e+17 ohm | IEC 60093 |
Ineos ABS Lustran® M205FC ABS Pellets, Injection Molding Grade Injection Molding grade for medical applications (e.g. inhalers, roller clamps, spikes, etc.)/ Biocompatible with up to 30 days human contact duration according to USP Class VI and ISO 10993-1. Food.. |
|||
Surface Resistance | >= 2.00e+17 ohm | >= 2.00e+17 ohm | |
Ineos Barex® 210 E Acrylonitrile-Methyl Acrylate Copolymer Extrusion Grade. Barex® Resins are available in either natural or blue tint. Barex® 210E is most commonly used for thermoformed sheet applications. |
|||
Surface Resistance | 2.00e+17 ohm | 2.00e+17 ohm | IEC 60093 |
Ineos ABS Lustran® Ultra 4105 ABS Pellets (Polycarbonate-modified), Medium High Heat Grade Lustran® Ultra 4105 is medium high heat grade with superior impact resistance. It is PC-modified and has low emission. It is used for the production of molded plastic articles. |
|||
Surface Resistance | >= 2.00e+17 ohm | >= 2.00e+17 ohm | IEC 60093 |
Styrolution Novodur® M205FC ABS Novodur HD M205FC is an injection molding grade especially suitable for medical applications providing enhanced stiffness.Information provided by Styrolution |
|||
Surface Resistance | 2.00e+17 ohm | 2.00e+17 ohm | IEC 60093 |
Polyplastics Duranex® 2002 Polybutylene Terephthalate (PBT), Standard DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Surface Resistance | 2.00e+17 ohm | 2.00e+17 ohm | IEC 60093 |
Polyplastics Duranex® 2002U Polybutylene Terephthalate (PBT), Weather resistance DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Surface Resistance | 2.00e+17 ohm | 2.00e+17 ohm | IEC 60093 |
Polyplastics Duranex® 733LD Polybutylene Terephthalate (PBT), Low warpage, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Surface Resistance | 2.00e+17 ohm | 2.00e+17 ohm | cured 21 days, 22°C; 45-55% RH; IEC 60093 |
Loctite® 5920™ RTV Silicone Sealant LOCTITE® 5920™ is a moisture-curing, non-corrosive silicone. The thixotropic nature of LOCTITE® 5920™ reduces the migration of liquid product after application to the substrate. It has been desi.. |