Polymer Property : Surface Resistance = 2.30e+16 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 2.30e+16 ohm
2.30e+16 ohm
ROA; IEC 60093
SABIC Innovative Plastics Ultem ATX153R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Surface Resistance 2.30e+16 ohm
2.30e+16 ohm
ROA; IEC 60093
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Surface Resistance 2.30e+16 ohm
2.30e+16 ohm
ROA; IEC 60093
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..