Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 2.72e+12 ohm | 2.72e+12 ohm | ohm/cm |
Pyrotek NAD-1000 High Temperature Engineering Board NAD-1000 is a high density calcium silicate board reinforced with selected fibers to produce excellent thermal characteristics and dimensional stability up to 1000°C. NAD-1000 retains high strengt.. |