Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 2.90e+10 ohm | 2.90e+10 ohm | |
Covestro Desmopan® 487 Thermoplastic Polyurethane Desmopan 487 is a TPU on the basis of a special ester.Applications: Seals, gear wheels, shoe heels, engineering components in the automotive sector.Information provided by Bayer.As of 1 September 20.. |