Surface Resistance 3.16e+14 ohm
3.16e+14 ohm
E24/125; IPC TM-650 2.5.17.1
Arlon AD1000 PTFE/Woven Fiberglass/Ceramic Filled Laminate for Microwave Printed Circuit Boards
Only Woven Glass Reinforced PTFE/Ceramic with Dk of 10.2 or greaterHigh Copper Peel Strength allows for thinner etched line widthsLowest insertion loss availableLarger Panel sizes availableLow moist..