Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | >= 4.00e+16 ohm | >= 4.00e+16 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics Cycoloy® CY6414 PC (Asia Pacific) |
|||
Surface Resistance | >= 4.00e+16 ohm | >= 4.00e+16 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics Cycoloy® CY6414 PC (Europe-Africa-Middle East) Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering high heat for application in appliances, lighting and electrical market. |
|||
Surface Resistance | <= 4.00e+16 ohm | <= 4.00e+16 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics Cycoloy® CY6414 PC+ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Surface Resistance | 4.00e+16 ohm | 4.00e+16 ohm | IEC 60093 |
Polyplastics Duranex® 3216 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Surface Resistance | 4.00e+16 ohm | 4.00e+16 ohm | IEC 60093 |
Polyplastics Duranex® 3405 Polybutylene Terephthalate (PBT), Standard, 45% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Surface Resistance | 4.00e+16 ohm | 4.00e+16 ohm | IEC 60093 |
Polyplastics Duracon® GH-25D Acetal Co-polymer (POM), GF 25% reinforced, High flow, High strength, High rigidity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |