Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 4.19e+14 ohm | 4.19e+14 ohm | Insulation Resistance, Condition A, ASTM D257 |
Glastic BMC SLC-1000 Glass-Reinforced Polyester Data provided by Glastic Corporation.Medium strength, V-0, adjustable shrinkage. |