Polymer Property : Surface Resistance = 4.20e+14 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 4.20e+14 ohm
4.20e+14 ohm
ASTM D257
SABIC Innovative Plastics NORYL LTA1350 PPE+PS
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Surface Resistance 4.20e+14 ohm
4.20e+14 ohm
ROA; IEC 60093
SABIC Innovative Plastics NORYL LTA1350 PPE+PS
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Surface Resistance 4.20e+14 ohm
4.20e+14 ohm
ASTM D257
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Asia Pacific)
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Surface Resistance 4.20e+14 ohm
4.20e+14 ohm
ROA; IEC 60093
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Asia Pacific)
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Surface Resistance 4.20e+14 ohm
4.20e+14 ohm
ASTM D257
SABIC Innovative Plastics NORYL LTA5020 PPE+PS
Noryl* LTA5020 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Surface Resistance 4.20e+14 ohm
4.20e+14 ohm
ASTM D257
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Europe-Africa-Middle East)
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Surface Resistance 4.20e+14 ohm
4.20e+14 ohm
ROA; IEC 60093
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Europe-Africa-Middle East)
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..