Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 4.20e+15 ohm | 4.20e+15 ohm | Cond. A; IPC 2.5.17.1 |
Rogers Corporation RO4003C Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil RO4000® Series High Frequency Circuit Materials are glass-reinforced hydrocarbon and ceramic (not PTFE) laminates with TICER™ TCR® Thin Film Resistor Foils. These laminates are designed for perf.. |