Polymer Property : Surface Resistance = 4.80e+14 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 4.80e+14 ohm

@Temperature 70.0 °C
4.80e+14 ohm

@Temperature 158 °F
7 days water immersion; IEC 60093
Lucobit Lucofin® 7410 HFFR EBA MDH Cable Sheathing
Lucofin® 7410 HFFR is a thermoplastic, halogen free flame retardant and low smoke compound for the insulation and/ or sheathing of cables. This grade is based on ethylene butyl acrylate (EBA) and..