Electrical Properties Metric English Comments
Surface Resistance 1e+05 - 5.00e+7 ohm
1e+05 - 5.00e+7 ohm
ASTM D257
PolyOne Edgetek® MLS-195A Polysulfone Alloy - ESD Material  (discontinued **)
Data provided by PolyOne.
Surface Resistance 1e+05 - 5.00e+7 ohm
1e+05 - 5.00e+7 ohm
ASTM D257
PolyOne Edgetek® ES-06CF-09GF/000 RED Polyethersulfone - 6% Carbon - 9% Glass Fiber Reinforced - ESD Applications &
Data provided by PolyOne.