Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 5.30e+15 ohm | 5.30e+15 ohm | ASTM D257 |
Arkema Group Orgalloy® RS 6630 Polyamide 6.6 Alloy 30% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group |