Electrical Properties Metric English Comments
Surface Resistance 6.00e+11 ohm
6.00e+11 ohm
ASTM D257
Rogers Corporation Poron® 4701-30-15 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..
Surface Resistance 6.00e+11 ohm
6.00e+11 ohm
ASTM D257
Rogers Corporation Poron® 4701-30-20 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..
Surface Resistance 6.00e+11 ohm
6.00e+11 ohm
ASTM D257
Rogers Corporation Poron® 4701-30-30 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4..
Surface Resistance 6.00e+11 ohm
6.00e+11 ohm
ASTM D249
PlastxWorld CEVIAN® EG506 ABS
Inherently Static Dissipative and Glass Fiber reinforced ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by Plastx..
Surface Resistance 6.00e+11 ohm
6.00e+11 ohm
Covestro Desmopan® 588 Thermoplastic Polyurethane
Desmopan 588 is a TPU on the basis of a special ether with good microbe-resistance.Applications: Cable sheathing, hoses, profiles.Information provided by Bayer.As of 1 September 2015, Bayer Material..
Surface Resistance 6.00e+11 ohm
6.00e+11 ohm
Covestro Desmopan® 786 Thermoplastic Polyurethane
Desmopan 786 is a TPU on the basis of a special carbonate with very good microbe-resistance.Applications: Tabular films, films, profiles.Information provided by Bayer.As of 1 September 2015, Bayer M..