Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 6.50e+10 ohm | 6.50e+10 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC (Asia Pacific) LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |