Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 4.0 - 7.0 ohm | 4.0 - 7.0 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON MX01739C PP LNP* SAT-KON* MX01739C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System. |