Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 7.80e+11 ohm | 7.80e+11 ohm | IEC 93 |
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex |