Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 760000 ohm | 760000 ohm | ASTM D257 |
PolyOne Stat-Tech™ ST5220-0004 CP4D EG Black Polypropylene Impact Copolymer (PP Impact Copolymer) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |