Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | >= 8.00e+14 ohm | >= 8.00e+14 ohm | |
CEN® Electronic Material CN Polyimide Film, 2 Mil Thickness CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca.. |
|||
Surface Resistance | >= 8.00e+14 ohm | >= 8.00e+14 ohm | ASTM D257 |
CEN® Electronic Material CV Polyimide Film, 2 Mil Thickness CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup.. |