Electrical Properties Metric English Comments
Surface Resistance <= 842 ohm
<= 842 ohm
ASTM D257
Ensinger Tecatron® XP-85 Compression Molded PPS Compound, with 30% Carbon Fiber
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p..