Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+8 - 9.00e+14 ohm | 1.00e+8 - 9.00e+14 ohm | Average value: 8.27e+13 ohm Grade Count:11 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |