Polymer Property : Surface Resistance = 9.00e+14 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 9.00e+14 ohm
9.00e+14 ohm
Covestro Desmopan® 372 Thermoplastic Polyurethane
Desmopan 372 is a TPU on the basis of a special ester.Applications: Transport rolls, technical automotive parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separa..
Surface Resistance 9.00e+14 ohm
9.00e+14 ohm
Covestro Texin® 270 Urethane Thermoplastic Elastomer
Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop..