Polymer Property : Surface Resistance = 9.00e+9 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 9.00e+9 - 4.00e+11 ohm
9.00e+9 - 4.00e+11 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-LOY 63000CTC PC+POLYESTER (Asia Pacific)
A permanent antistatic PC-Alloy compound that features transparency and superior cleanliness for advanced semiconductor packaging applications
Surface Resistance 9.00e+9 ohm
9.00e+9 ohm
12% RH; ESD S11.11
Lubrizol Stat-Rite® M-809 Static Control Acrylic
Stat-Rite® M-809 is a static dissipative Acrylic alloy. Stat-Rite® M-809 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protec..