Polymer Property : Electrical Resistivity = 0.0000310 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000310 ohm-cm

@Temperature 100 °C
0.0000310 ohm-cm

@Temperature 212 °F
ATI Allegheny Ludlum K12® Dual Hardness Steel
This is a roll bonded, dual hardness armor plate consisting of a high hardness front side to break up or flatten incoming projectiles while the back side functions to capture the projectile.The comp..