Polymer Property : Electrical Resistivity = 0.0000960 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, 1.6 mm sheet
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, 12.7-50.8 mm bar
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, 19.1 mm thick plate, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, 6.3-38.1 mm plate
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, aged 1000 hours at 204°C (400°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, aged 1000 hours at 316°C
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, aged 1000 hours at 427°C (800°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, aged 1000 hours at 538°C (1000°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, aged 1000 hours at 649°C (1200°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, aged 1000 hours at 760°C (1400°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, aged 1000 hours at 871°C (1600°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, aged 1000 hours at 982°C
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, all-weld metal, GMAW weld (short)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, all-weld metal, GMAW weld (spray)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, all-weld metal, GTAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, all-weld metal, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, mill annealed
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, plate, GMAW weld (short)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 300 °C
0.0000960 ohm-cm

@Temperature 572 °F
Haynes Ultimet® alloy, plate, GMAW weld (spray)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 600 °C
0.0000960 ohm-cm

@Temperature 1110 °F
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel
A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 600 °C
0.0000960 ohm-cm

@Temperature 1110 °F
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel
W400 VMR is a low silicon, chromium-vanadium hot work tool steel which has been vacuum remelted to obtain the highest uniformity, the best cleanliness of tool steel. The material is characterized:E..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 600 °C
0.0000960 ohm-cm

@Temperature 1110 °F
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel
W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to ..
Electrical Resistivity 0.0000960 ohm-cm

@Temperature 600 °C
0.0000960 ohm-cm

@Temperature 1110 °F
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel
Properties:Hot work tool steel featuring excellent hot tensile properties, high hot wear resistance, adequate toughness and heat checking resistance, adequate toughness and heat checking; admits wat..