Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0001137 ohm-cm @Temperature 22.0 °C |
0.0001137 ohm-cm @Temperature 71.6 °F |
|
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy INCONEL® alloy MA 758 is an oxide-dispersion-strengthened (ODS) nickel-chromium superalloy, made by mechanical alloying. It is a development of the well-established aerospace superalloy, INCONEL.. |