Polymer Property : Electrical Resistivity = 0.0001299 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.0001299 ohm-cm

@Temperature 200 °C
0.0001299 ohm-cm

@Temperature 392 °F
Haynes 282® Nickel Alloy Autogenously Welded Sheet
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Electrical Resistivity 0.0001299 ohm-cm

@Temperature 1000 °C
0.0001299 ohm-cm

@Temperature 1830 °F
Haynes 282® Nickel Alloy Autogenously Welded Sheet
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Electrical Resistivity 0.0001299 ohm-cm

@Temperature 200 °C
0.0001299 ohm-cm

@Temperature 392 °F
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Electrical Resistivity 0.0001299 ohm-cm

@Temperature 1000 °C
0.0001299 ohm-cm

@Temperature 1830 °F
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Electrical Resistivity 0.0001299 ohm-cm

@Temperature 200 °C
0.0001299 ohm-cm

@Temperature 392 °F
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Electrical Resistivity 0.0001299 ohm-cm

@Temperature 1000 °C
0.0001299 ohm-cm

@Temperature 1830 °F
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Electrical Resistivity 0.0001299 ohm-cm

@Temperature 200 °C
0.0001299 ohm-cm

@Temperature 392 °F
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Electrical Resistivity 0.0001299 ohm-cm

@Temperature 1000 °C
0.0001299 ohm-cm

@Temperature 1830 °F
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Electrical Resistivity 0.0001299 ohm-cm

@Temperature 200 °C
0.0001299 ohm-cm

@Temperature 392 °F
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Electrical Resistivity 0.0001299 ohm-cm

@Temperature 1000 °C
0.0001299 ohm-cm

@Temperature 1830 °F
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Electrical Resistivity 0.0001299 ohm-cm

@Temperature 200 °C
0.0001299 ohm-cm

@Temperature 392 °F
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..
Electrical Resistivity 0.0001299 ohm-cm

@Temperature 1000 °C
0.0001299 ohm-cm

@Temperature 1830 °F
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..