Electrical Properties Metric English Comments
Electrical Resistivity 0.000135 ohm-cm

@Temperature 500 °C
0.000135 ohm-cm

@Temperature 932 °F
Haynes 282® Nickel Alloy Autogenously Welded Sheet
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Electrical Resistivity 0.000135 ohm-cm

@Temperature 500 °C
0.000135 ohm-cm

@Temperature 932 °F
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Electrical Resistivity 0.000135 ohm-cm

@Temperature 500 °C
0.000135 ohm-cm

@Temperature 932 °F
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Electrical Resistivity 0.000135 ohm-cm

@Temperature 500 °C
0.000135 ohm-cm

@Temperature 932 °F
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Electrical Resistivity 0.000135 ohm-cm

@Temperature 500 °C
0.000135 ohm-cm

@Temperature 932 °F
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Electrical Resistivity 0.000135 ohm-cm

@Temperature 600 °C
0.000135 ohm-cm

@Temperature 1110 °F
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Electrical Resistivity 0.000135 ohm-cm

@Temperature 600 °C
0.000135 ohm-cm

@Temperature 1110 °F
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Electrical Resistivity 0.000135 ohm-cm

@Temperature 600 °C
0.000135 ohm-cm

@Temperature 1110 °F
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Electrical Resistivity 0.000135 ohm-cm

@Temperature 600 °C
0.000135 ohm-cm

@Temperature 1110 °F
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Electrical Resistivity 0.000135 ohm-cm

@Temperature 600 °C
0.000135 ohm-cm

@Temperature 1110 °F
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Electrical Resistivity 0.000135 ohm-cm

@Temperature 600 °C
0.000135 ohm-cm

@Temperature 1110 °F
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Electrical Resistivity 0.000135 ohm-cm

@Temperature 500 °C
0.000135 ohm-cm

@Temperature 932 °F
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..
Electrical Resistivity 0.000135 ohm-cm

@Temperature 600 °C
0.000135 ohm-cm

@Temperature 1110 °F
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C)
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..