Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Electrical Resistivity = 2.00e+15 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 2.00e+15 ohm-cm

@Temperature 25.0 °C
2.00e+15 ohm-cm

@Temperature 77.0 °F
Abatron AboCast 8-5/Abocure 8-5 Epoxy  (discontinued **)
2-part solvent-free dielectric epoxy casting compound.Processing: 100/80.5 ratio (pbw); Gel time, 100 g (3.5 oz.): 300 minutes; cures in 3 weeks at 25°C (77°F).Applications: solventless casting, a..
Electrical Resistivity 2.00e+15 ohm-cm

@Temperature 25.0 °C
2.00e+15 ohm-cm

@Temperature 77.0 °F
Abatron AboCast 8-6/Abocure 8-6 Epoxy  (discontinued **)
2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 1 lb. (2.2 kg): 115 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F)...
Electrical Resistivity 2.00e+15 ohm-cm

@Temperature 25.0 °C
2.00e+15 ohm-cm

@Temperature 77.0 °F
Abatron AboCast 8-7/Abocure 8-7 Epoxy  (discontinued **)
2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 1 lb. (2.2 kg): 125 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F)...
Electrical Resistivity 2.00e+15 ohm-cm

@Temperature 25.0 °C
2.00e+15 ohm-cm

@Temperature 77.0 °F
Abatron AboCast 8-10/Abocure 8-10 Epoxy  (discontinued **)
2-part solvent-free dielectric epoxy casting compound.Processing: 100/35 ratio (pbw); Gel time, 1 lb. (2.2 kg): 45 minutes; cures in 6 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F).Ap..
Electrical Resistivity 2.00e+15 ohm-cm

@Temperature 25.0 °C
2.00e+15 ohm-cm

@Temperature 77.0 °F
Abatron AboCast 8-11/Abocure 8-11 Epoxy  (discontinued **)
2-part solvent-free dielectric epoxy casting compound.Processing: 100/35 ratio (pbw); Gel time, 100 g (3.5 oz.): 93 minutes; cures in 3 weeks at 25°C (77°F).Applications: solventless casting, adhe..
Copyright © lookpolymers.com All Rights Reserved