Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 3.00e+15 ohm-cm @Temperature 25.0 °C |
3.00e+15 ohm-cm @Temperature 77.0 °F |
|
Abatron AboCast 8-2/Abocure 8-2 Epoxy
(discontinued **) 2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 100 g (3.5 oz.): 265 minutes; cures in 3 weeks at 25°C (77°F).Applications: solventless casting, adh.. |
|||
Electrical Resistivity | 3.00e+15 ohm-cm @Temperature 25.0 °C |
3.00e+15 ohm-cm @Temperature 77.0 °F |
|
Abatron AboCast 8-17/Abocure 8-17 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/35.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 123 minutes; cures in 2 weeks at 25°C (77°F).Applications: solventless c.. |