Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 3.60e+15 ohm-cm @Temperature 25.0 °C |
3.60e+15 ohm-cm @Temperature 77.0 °F |
|
Abatron AboCast 8-9/Abocure 8-9 Epoxy
(discontinued **) 2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 100 g (3.5 oz.): 480 minutes; cures in 3 weeks at 25°C (77°F).Applications: solventless casting, adh.. |
|||
Electrical Resistivity | 3.60e+15 ohm-cm @Temperature 25.0 °C |
3.60e+15 ohm-cm @Temperature 77.0 °F |
|
Abatron AboCast 8-3/Abocure 8-3 Epoxy 2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 100 g (3.5 oz.): 265 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F).. |