Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 40.0 ohm-cm @Temperature 90.0 °C |
40.0 ohm-cm @Temperature 194 °F |
ASTM D991 |
Borealis Supersmooth™ LE0500 Crosslinkable Semiconductive Shielding Compound Supersmooth LE0500 is a crosslinkable compound recommended as conductor and bonded insulation shielding for crosslinked polyethylene insulation. Supersmooth LE0500 is based on an ethylene butyl acry.. |