Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 6.00e+11 ohm-cm @Temperature 65.6 °C |
6.00e+11 ohm-cm @Temperature 150 °F |
|
Abatron AboCast 8-7/Abocure 8-7 Epoxy
(discontinued **) 2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 1 lb. (2.2 kg): 125 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F)... |
|||
Electrical Resistivity | 6.00e+11 ohm-cm @Temperature 65.6 °C |
6.00e+11 ohm-cm @Temperature 150 °F |
|
Abatron AboCast 8-17/Abocure 8-17 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/35.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 123 minutes; cures in 2 weeks at 25°C (77°F).Applications: solventless c.. |