Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+14 ohm @Temperature 23.0 °C |
1.00e+14 ohm @Temperature 73.4 °F |
50% r.h.; DIN 53482 or VDE 0303/part 3 or ASTM D257 |
Mitsubishi Hostaphan® WN, 190 micron Nominal Thickness Translucent White Polyethylene Terephthalate Film Hostaphan® WN is a white film made of polyethylene terephthalate (PET) and is well suited for electrical insulating of machines and appliances. The high dielectric strength and large volume resis.. |
|||
Surface Resistance | 1.00e+14 ohm @Temperature 23.0 °C |
1.00e+14 ohm @Temperature 73.4 °F |
ASTM D257 |
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**) Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers |
|||
Surface Resistance | 1.00e+14 ohm @Temperature 23.0 °C |
1.00e+14 ohm @Temperature 73.4 °F |
IEC 60093 |
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**) Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers |