Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | >= 1.00e+17 ohm @Temperature 25.0 °C |
>= 1.00e+17 ohm @Temperature 77.0 °F |
DC100V; ASTM D257 |
UBE UPILEX 25S (25 micron) Polyimide Film Description: UPILEX, the ultra-high heat-resistant polyimide film, is the product of the polycondensation reaction between biphenyltetracarboxylic dianhydride (BPDA), of which process Ube Industries.. |