Electrical Properties | Metric | English | Comments |
---|---|---|---|
Track Resistance | >= 1.20e+6 sec | >= 1.20e+6 sec | Wet, 2.5 KV; ASTM D2303 |
Master Bond EP112 Low Viscosity Heat Curing Cycloaliphatic Epoxy Adhesive Master Bond Polymer System EP112 is a solventless, low viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor and indoor electrical & e.. |