Electrical Properties | Metric | English | Comments |
---|---|---|---|
Track Resistance | >= 16.67 sec | >= 16.67 sec | |
Bulk Molding Compounds BMC SLC 2000 Glass Reinforced Polyester BMC SLC 2000 is a medium strength, low-cost, glass reinforced polyester compound with adjustable shrinkage. Ideal for circuit breakers, motor switch housings, fuse holders, brush holders, standoff i.. |