Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 1.07e+10 ohm @Time 86400 sec |
1.07e+10 ohm @Time 24.0 hour |
Control |
Indium Corp. #2212-10 Wave Solder Flux Features:High solids, no-clean, rosin containing fluxMeet J-STD-004A type ROL1 an dQQS-571F type RMAGreater heat stability than low solids fluxesDesigned for soldering thick and massive circuit boar.. |