Electrical Properties Metric English Comments
Magnetic Maximum Energy Product, BH 16 - 18 MGOe
16 - 18 MGOe
Ceradyne SEMICORE® S1-5B MMPA 16/18 SmCo5 Samarium Cobalt Magnet
Magnetic alignment parallel to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Her..
Magnetic Maximum Energy Product, BH 16 - 20 MGOe
16 - 20 MGOe
Ceradyne SEMICORE® S2-17C Specials Sm2 (CoFeCuZr)17 Samarium Cobalt Magnet
Applications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Hermetic magnetic couplings to replace shaft seal..