Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Maximum Energy Product, BH | 3.9 MGOe | 3.9 MGOe | |
Alliance A-5S Alnico Magnetic Material |
|||
Magnetic Maximum Energy Product, BH | 3.9 MGOe | 3.9 MGOe | |
Alliance C-8B Strontium Ferrite Ceramic Magnetic Material |