Polymer Property : Comparative Tracking Index = 155 V Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Comparative Tracking Index 155 V

@Thickness 3.17 mm
155 V

@Thickness 0.125 in
ASTM D3638
Industrial Laminates/Norplex NP310 Cotton Fabric
Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Thickness Tested: 0.062, 0.125", and 0.500".
Comparative Tracking Index 155 V
155 V
IEC test
Toyobo TS301 PPS, 30% Glass Fiber Reinforced
Key Feature: Excellent impact resistance, high flowHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo..