Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 215 V | 215 V | IEC test |
Toyobo TS201 PPS, Glass Fiber/Mineral Reinforced Key Feature: Standard high stiffness - used for metal replacementHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology devel.. |
|||
Comparative Tracking Index | 215 V | 215 V | IEC test |
Toyobo Vylopet® EMC630 PET/PBT Blend Key Feature: Flame retardant V-0 UL 94 classApplications: general and high rigidity componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, go.. |