Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 265 V | 265 V | IEC test |
Toyobo Vylopet® EMC317R Glass Reinforced Polyester, Standard Grade Key Feature: UL-94 classApplications: Glossy surface componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, ch.. |